Glassing the hull
I have now started the process of fibre-glassing the hull. I have used two layers of 125g/sqm (4oz) glass, and both epoxied at the same time. After applying the 'wetting out' coat with a wooden spatula (probably a poor choice!), I applied two top coats using a foam roller. My objective is to just cover the weave of the cloth...